Anybody ever try this?

AKE of nitric acid 4 ozs.; muriatic acid, ? oz. Mix togetner. Now cover the place you wish to write on with beeswax, the beeswax to be warm when applied. When it is cold, write your name with a sharp instrument. Be sure to write so that the steel is discernible in the name. Now apply the mixture with a feather, well filling each letter. Let the mixture remain about five minutes or more, according to the depth desired; then wash off the acid; water will stop the process of the same. When the wax is removed, the inscription is plain.