thanks jim I just took a look and it seems prity good as far as the description goes I still don't know everything about the ingredients I do know stainless needs to have 10.5% chromium right? the 3-v has 7.5 but that's still enough to give it resistance to rust right. jim do you know anything about positive pressure quench (or any where I can get some info on it) ray had described it a lil but I cant remember the details (I tried to find the thread he explained it and couldn't find it) but I also don't think we talked about it in detail so I definitely need to get some more info on that as I was looking at a few different steels and a lot of them have this as a quench option and I would like to do testing on a couple different ways if I start using a new steel. I did some searching on positive pressure quenching and really could find much and nothing on how its actually accomplished.
|
Tags |
1095, art, blade, blades, brass, cryo, files, grind, harden, heat, home, hot, knife, knives, make, material, metal, problem, rod, scale, small, steel, store, supply, temper |
Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
Thread Tools | |
Display Modes | |
|
|
Similar Threads | ||||
Thread | Thread Starter | Forum | Replies | Last Post |
liquid nitrogen dewar | dtec1 | The Newbies Arena | 10 | 08-19-2016 04:46 AM |
Liquid Nitrogen Dewar | Andrew Garrett | Heat Treating and Metallurgy | 4 | 02-01-2016 05:30 AM |
Liquid Nitrogen | ryano | The Newbies Arena | 7 | 09-12-2012 01:51 PM |
Liquid Nitrogen questions | dbalfa | Heat Treating and Metallurgy | 8 | 02-13-2010 07:40 AM |
looking for dewar for liquid nitrogen | kildar888 | Heat Treating and Metallurgy | 2 | 06-26-2007 10:27 PM |