Seems real similar to Sandvik 14C28N

Except for the minuscule amount of Vanadium at 0.079 and a slightly higher Carbon, 0.68 vs. 0.62 content they could be the same. I have no idea what such a small amount of Vanadium would accomplish, but they put it in there for some reason. I'm no expert on the Nitrogen bearing steels, but would recommend you call Peters HT in Meadville PA or call NJSB and ask how to HT this alloy. Here is a link to the Sandvik data sheet.