My experience with O1 Ray is with a kiln at 1475 it's a fair orange color and bright orange isn't going to be too much, the problem is only two minutes and how did he quench it. If he twirled the blade around it would warp and if he ground too much off it's going to be very prone to warp. Yes bright orange is a little too hot, but at least he didn't say yellowish orange.