01 should not be considered a "simple" simple steel due to the number of alloys in it, though it is often is addressed as such. 01 requires more than just a simple heat, quench, and temper HT if optimal results are wanted, and it should never be taken much beyond 1475? for the hardening quench due to the possibility of putting more carbon into solution than is really needed.