Quote:
Originally Posted by M&J
Checking back, how did it work?
|
Well, I tried etching on a scrap piece of 6-4 TI using my regular electrolyte and it was a mess. But I sort of expected that. I think the secret is in the electrolyte used.
I ordered the electrolyte recommended above from USA knifemaker and have it on hand but haven't had a chance to give it a try. I'm running a set of 5 stainless flipper folders for some folks and hope to get the blades heat treated this week. Then a couple of days to finish up and I'll be ready to start on the TI ones.
I want to give the logo etching a try before I go too far as I'd like to color anodize the TI folders and don't know how the logo etching and anodizing will interact. But that's why I save scraps for experimentation!
I'll try to remember to come back and let you know what I experience.